The EB 24 film creep tester has a digital ruler system including a line laser pointer for manual creep measurement of plastic.
The ruler is connected to the included computer via Bluetooth and the values are fed into a spreadsheet template which calculates the result and presents the graphs.
The air supply for EB 24 requires external air. Elastocon offers a silent air compressor, EA 01, if compressed air is missing.
Standards
- ISO 188
- IEC 811
- other equivalent standards
Temperature range
+40 °C to +200 °C
Important specifications
- Temperature variation in time ± 0,25 °C
- Temperature variation in space ± 0,5 %
- Special design with controlled air exchange rate and low air speed
- Has a flow meter that can be set between 3 to 20 changes per hour
- The air speed is low and is dependent on the air exchange rate only
- Temperature indicator with sensor in the inner chamber
- Temperature controller with 0,1 °C set point
- Fixed over temperature fuse
- Cooling channels in the casing for low surface temperature
- Run time meter
- Countdown timer
- Door sensor to turn off heat and illumination when door is opened
- 4 glass window in the door
- Digital ruler and line laser to measure the samples connected to the computer via bluetooth
Included accessories
- Computer (Windows) with necessary software
- Hooks to hang 10 test pieces, 25 × 100 mm (thickness of test specimens max 3,5 mm)
- 10 sets of grips to attach to the test pieces together with weights (1,3 kg and 2,3 kg)
- Manual in English
- Stylus pen for the instrument touch screen
- Accredited calibration including certificate
Optional accessories
- EB-P – Ramp function for cycling temperature settings in the PLC. Observe that cooling of the oven will be natural cooling due to ambient temperature (very slow and non-controlled).
- EC 11 – Monitor Plus software.
- ED 06 – Uninterruptible power supply (UPS), recommended for the included computer to eliminate disturbances from power failures up to 30 minutes.
- ED 07.01-x – network cable in different lengths: 3, 5, and 10 m (replace x in the article number with the desired length).
- EA 01 – Silent air compressor, 105 l/min – read more about EA 01 here
More information
Product brochure: Elastocon – Stress relaxation and creep systems.pdf
Watch our video about the EB 24 film creep tester