Stress relaxation rigs
Elastocon's EB 02 is a relaxation rig for continuous stress relaxation measurements of rubber in both compression and tension according to ISO 3384, ISO 6914 method A and ASTM D6147. The rig works together with the cell ovens EB 21, EB 22, EB 38 and the programmable temperature cycling cell ovens EB 21LTHTP and EB 17, or with our temperature boxes for test at room temperature and below.
The EB 02 relaxation rigs are available in different options for continuous stress relaxation measurements of rubber in both compression and tension according to ISO 3384, ISO 6914 method A, ASTM D6147 and SAE J2979.
The high force relaxation rig EB 02HF is used for testing of stress relaxation with high forces up to 45 kN (45 000 N), according to ISO 3384.