The EB 02.14-x amplifier box EB 02.14-x connects the stress relaxation rigs to a computer for acquisition of the force and temperature data in relaxation testing of rubber.
The amplifier box communicates via a network connection. This means that the amplifier can be directly connected to the network connector on a computer, or anywhere in a local ethernet network.
The box can also have up to 24 channels or connect 12 relaxation rigs. X = number of rigs that can be connected to the amplifier box, available in sizes: 2, 4, 6, 8 or 12 rigs per box.
Important specifications
Input Pt 100
- Connection type: 3 wire
- Temperature range: -200 to +850 °C
- Resolution: 0,1 °C
- Conversion time: 320 ms
- Measuring error (25 °C): ± 0,2 % of full range
- Bit width, bits: 2 × 16
Load Cell input
- Signal voltage, Ud, mV: -16 till +16
- Signal voltage, Uref, V: -10 till +10
- Resolution: 16 bits
- Conversion time: 250 ms
- Measuring error, %: 0,1 of full range
- Bit width: 16 bits
Communication
- Transmission medium: Twisted pair S-UTP 100 ¤ cat5
- Buscoupler connection: RJ45
- Max length of fieldbus segment: 100 m between hubstation EB 02.14
- Baud rate: 10 mbit/s
- Protocols: ModBus/TCP, HTTP, bootp ModBus, UDP
More information
Product brochure: Elastocon – Stress relaxation and creep systems.pdf
Related articles