The DSC 4000 offers dependable performance and quality results. This single-furnace, heat flux DSC is designed to run all your routine applications and includes an easy-to-load vertical furnace that is resistant to oxygen and chemical corrosion.
The DSC 4000 is a compact workhorse that performs like a champion. It’s the ideal solution for a wide range of routine applications in the academic, polymer and pharmaceutical markets.
Differential scanning calorimetry (DSC) is a thermoanalytical technique in which the difference in the amount of heat required to increase the temperature of a sample and reference is measured as a function of temperature.
Graphs from differential scanning caloriemetry (DSC) can be used in the classification of melting intervals and phase transformations.
Typical applications for the DSC 4000
- QA/QC testing
- Undergraduate teaching practicals
- Evaluating additives for plastic lifetime optimization
- Ideal for Oxidation Induction Test (OIT)
Features and benefits
- Integrated mass flow controller for convenient gas control and switching
- Fast 45-position autosampler option for reliable unattended operation
- Portable cooling device (PCD) for cost-effective operation at low temperature
- Efficient, easy-to-clean nickel chromium sample plate
More information
Data sheet: PerkinElmer DSC 4000-6000.pdf