The EB 02.01P airtight container can be used up to a pressure of 3 bar together with the stress relaxation rigs EB 02 and EB 02AP for compression testing of rubber in liquids at temperatures up to +150 °C, according to ISO 3384.
This container makes it possible to test samples in coolants under pressure. The upper compression plate has a hole for the liquid to circulate through.
A pressure gauge, EB 02.01P6, is also available as an option for this container.
Important specifications
- Temperature range: +5 to 150 °C
- Diameter: 90 mm
- Height: 95 + 25 mm
- Weight: 1,1 kg
- Material: Stainless steel
- Seals: FPM (default) or EPDM (option)
Consumables
- EB 02.01P1, set of 6 O-rings, FPM for EB 02.01P
- EB 02.01P2, set of 6 O-rings, EPDM (Peroxide cured) for EB 02.01P