The EB 02.01 container is used with the stress relaxation rig EB 02 for compression testing of rubber in liquids at temperatures up to +200 °C, according to ISO 3384.
The EB 02.01 container makes it possible to test samples in liquids such as coolants, oil, water etc. The container has a hole for the liquid to circulate through.
Note: This container is not air tight.
Important specifications
- Maximum temperature: +200 °C
- Diameter: 90 mm
- Height: 95 mm
- Weight: 1 kg
- Material: Stainless steel