The EB 02.25 low temperature box is almost the same as EB 02.08, except that it is equipped with water cooling by tap water. It is used for stress relaxation testing of rubber in room temperature to avoid variation in the load curve caused by temperature variation in the laboratory.
This cooling enables temperature range between +4 to +40 °C. Tap water temperature cannot exceed +18 °C. The capacity of the box is 8 stress relaxation rigs. It can also be used for conditioning test pieces at 23 °C.
Important specifications
- Temperature range: +4 to +40 °C (lowest temperature is depending of the tap water temperature)
- Nominal temperature: 23 °C
- Temperature variation in time: ± 0,5 °C
- Temp. variation in space: ± 1,0 %
- Temperature reduction, below ambient: minimum 12 °C
Included accessories
- Manual in English
- Accredited calibration including certificate
- Software for change of the default temperature