Room temperature box EB 02.08

The EB 02.08 room temperature box is used for stress relaxation testing of rubber in room temperature to avoid variation in the load curve caused by temperature variation in the laboratory.

The capacity of the box is 8 stress relaxation rigs. It can also be used for conditioning test pieces at 23 °C.

Click image to enlarge. This graph shows a test run with and without the EB 02.08 room temperature box when testing at 23 °C. The blue curve are the rigs without the box and for the red curve the box is used. The green curve is the room temperature.

Important specifications

  • Temperature range: +10 to +40 °C (lowest temperature is depending of ambient temperature)
  • Nominal temperature: 23 °C
  • Temperature variation in time: ± 0,25 °C
  • Temperature variation in space: ± 1,0 %
  • Temperature reduction, below ambient: minimum 12 °C

Included accessories

  • Manual in English
  • Accredited calibration including certificate
  • Software for change of the default temperature

More information

Product brochure: Elastocon – Stress relaxation and creep systems.pdf


Manufacturer: Elastocon